← All insights

Abrasion and Scratch Resistance in Synthetic Leather

A synthetic leather can withstand repeated rubbing yet show a visible mark from one sharp contact. Another may resist a light scratch while losing its finish under continuous friction.

Abrasion resistance and scratch resistance address different damage mechanisms. A professional specification defines both where relevant and includes the appearance changes the customer will consider unacceptable.

How Abrasion and Scratching Differ

Abrasion involves repeated surface wear from friction against another material. A scratch involves localized contact that can deform, mark, or cut the surface.

The distinction is useful even when the damage overlaps. A bag may rub against clothing throughout the day and also encounter keys. A seat may experience clothing friction and occasional concentrated contact from a hard object.

A single durability result cannot represent all of these interactions.

Appearance Can Fail Before the Coating Wears Through

A surface can remain structurally intact while developing gloss change, grain flattening, color loss, or polishing. For a matte or printed product, these changes can determine acceptance before a hole appears.

Stahl’s coating portfolio treats scuffing, polishing, scratch resistance, and abrasion resistance as surface-performance concerns.[1] These are useful distinctions when defining a finished appearance.

Specify whether an acceptable result means no coating breakthrough, limited color change, acceptable gloss retention, or another observable endpoint.

Read Abrasion Results With the Full Test Conditions

A cycle count needs its method, abrasive medium, applied load, specimen preparation, and endpoint.

ISO 5470-2 addresses wet and dry abrasion of coated surfaces using a Martindale abrader.[2] Other procedures use different motions and contact conditions. Results should not be converted between methods without a validated basis.

Record the tested face and whether the result represents the original material, a cleaned sample, or an aged construction. Compare suppliers using the same protocol.

Make Scratch Evaluation Repeatable

An informal fingernail test can reveal a difference, but its force, angle, tip condition, and speed are uncontrolled.

For development screening, use a documented contact tool, load, movement, and evaluation procedure. Inspect both the immediate mark and any recovery after a defined period.

A removable transfer mark, permanent indentation, topcoat damage, and a cut through the coating should be recorded as different outcomes. Cleaning a mark away does not demonstrate the absence of underlying damage.

Include the Supporting Structure

The backing and cushioning beneath the surface affect how local contact is distributed. Test the material on the support used in the product when that support influences performance.

For an upholstered panel, compare a flat sheet with a panel wrapped over the intended foam and edge geometry. For a glove patch, assess the assembled fingertip and its bends.

These product-level trials complement material tests by exposing stress concentrations and construction effects.

AssessmentWhat it examinesWhat to define or record
AbrasionRepeated surface wear caused by friction.Method, abrasive medium, load, specimen preparation and endpoint.
Scratch or scuffLocalized contact that can mark, deform or cut the surface.Contact tool, load, movement, immediate mark and recovery period.
Appearance changeGloss change, grain flattening, color loss or polishing.The observable changes that make the finish unacceptable.
Product-level contactEffects of backing, cushioning, bends and edges.Intended support and assembled geometry, alongside material tests.
Separate the damage mechanisms before comparing results

Build a Balanced Durability Requirement

A useful test matrix can include:

  • Abrasion to a specified appearance or structural endpoint.
  • Scratch or scuff evaluation under a defined procedure.
  • Flexing around folds and seams.
  • Cleaning followed by repeat evaluation.
  • Aging relevant to the service environment.
  • Inspection of exposed edges and high-contact areas.

Do not convert a high abrasion count into a service-life promise. ACT specifically cautions that abrasion results are not reliable predictors of fabric lifespan.[3]

Select the material against the actual combination of contact, appearance, and maintenance conditions, then preserve the approved finish and construction in the production specification.

References

  1. Stahl. (n.d.). PolyMatte®: Scratch-resistant Matte Coatings for Synthetics and Leather.Technical resource · Accessed 6 November 2026.
  2. ISO. (2021). ISO 5470-2:2021 — Rubber- or plastics-coated fabrics: Abrasion resistance using a Martindale abrader.International standard · Accessed 6 November 2026.
  3. Association for Contract Textiles (ACT). (n.d.). Abrasion — High Traffic: Coated Fabrics, Indoor Use.Industry guideline · Accessed 6 November 2026.

← Back to insights